Micromeritics Gemini VI BET surface area analyser

Micromeritics Gemini VI Capabilities

A physical gas adsorption instrument used to estimate surface area by BET, mesopore and micropore distribution analyses and isotherm studies. 

  • Rapid twin-tube setup.
  • Single- and Multipoint BET surface area
  • Langmuir surface area
  • Pore volume and pore area distributions in the mesopore and macropore ranges by the BJH method using a variety of thickness equations including a user-defined, standard isotherm
  • Specific: 0.01 m2/g and higher
    Total: 0.1 m2 and higher, +\- 0.03 m2
    Pore Volume: 4 x 10-6 cm3/g and higher
  • Pore volume (distribution and total pore volume) in a user-defined pore size range
  • Micropore distribution by the MP-method and total micropore volume by the t-Plot and as Plot methods
  • Halsey, Harkins-Jura, Carbon Black STSA, Broekhoff-de Boer and user-entered thickness curves